LCD Cell Glass 이송용 도전성 PE Foam 간지(무가교, 전자선가교 타입)
| Properties | Unit | Value | Method |
|---|---|---|---|
| Sheet Resistance | Ohms per square | 10E6-9 | ASTM D257 |
| Surface Resistivity After Abrasion |
Ohms per square | 10E6-9 | ASTM D257 ASTM D1044 |
| Solvent Resist (Di water, IPA, Hexane) |
Surface Resistivity | No Charge | ASTM D543 |
| Properties | Unit | Value | Method |
|---|---|---|---|
| Apparent Density | g/cm sa | Over 0.12 | KSM3503 |
| Tribo Charge | V | Below 5 | |
| DecayTime | Sec | Below 0.1 | |
| Tensile strength | Kgf/cm2 | MD Over 15 TD Over 9 |
KSM3503 |
| Tear strength | Kgf/cm | MD Over 9 TD Over 4 |
KSM3503 |
| Hardness | F-type | 80 | KSM3503 |
| Elongation | % | MD Over 150 TD Over 120 |
KSM3503 |
| An anion Content F- CI- NO- Br- |
mg/cm2 | ND ND ND ND |
Ion Chromatography MDL 0.1mg/cm2 |
| Properties | Unit | Value | Method |
|---|---|---|---|
| Apparent Density | g/cm sa | Below 0.09 | KSM3503 |
| Tribo Charge | V | Below 5 | |
| DecayTime | Sec | Below 0.1 | |
| Tensile strength | Kgf/cm2 | MD Over 35 TD Over 25 |
KSM3503 1798:2002 |
| Tear strength | Kgf/cm | MD Over 25 TD Over 20 |
KSM3503 |
| Elongation | % | MD Over 40 TD Over 2 |
KSM3503 |
| An anion Content F- CI- NO- Br- |
mg/cm2 | ND ND ND ND |
Ion Chromatography MDL 0.1mg/cm2 |
전자제품 완제품 포장용 AI-PET PE Foam - Bag(방오.방습)
| Properties | Unit | Value | Method |
|---|---|---|---|
| Tensile strength | Kgf/cm2 | MD Over 4.2 TD Over 4.2 |
KSM3503 |
| Sealing strength | Kgf/cm2 | MD Over 4 TD Over 4 |
|
| Elongation | % | MD Over 85 TD Over 85 |
KSM3503 |
| Moisture Vaper Permeability |
g/cm2day | Below 0.5 | KSM3503 |
| Contact Angle | ° | Over 80 |